How to repair chips on the bathroom

How to repair chips on the bathroom

The chip of enamel covering on bathtub or sink is both deterioration in exterior, and the inconveniences arising in use. The first that comes to mind – to replace the spoiled thing. But you do not hurry. It is possible to try to repair enamel covering independently.

It is required to you

  • - abrasive paper;
  • - gasoline;
  • - acetone or alcohol;
  • - porcelain;
  • - mortar and pestle;
  • - epoxy glue;
  • - BF-2 glue;
  • - zinc white;
  • - Supertsement
  • - restorer of QULOSA enamel or BISON reducer;
  • - reducers "Svetlana", "Renesans", "Fantaziya";
  • - abrasive stone;
  • - vacuum cleaner.

Instruction

1. There are special materials by means of which it is possible to restore covering of bathtubs, sinks, washing, drying and dish washers, fridges, gas-fires, etc. The restorer of QULOSA enamel or BISON reducer is suitable for these purposes. Process the damaged surface abrasive paper. Wipe with gasoline, then dry. Put enamel layer. Let's dry out. Put still layer and leave for day. In 24 hours you will have brilliant, thermo-hydroresistant surface.

2. In the presence of considerable damages get the means intended for cardinal restoration of enamel covering – Svetlana, "Renesans", "Imagination". Special cleansers are included in the package with them. Process them the surface which is subject to restoration by means of abrasive stone before emergence of dense grid of scratches. Remove garbage with the vacuum cleaner and properly wash bathtub with hot water. Dry. Further act according to the instruction which is attached to reducer.

3. Easy and cheap way of restoration of surface – use of porcelain patch. Process the place of chip abrasive paper. Wipe with gasoline. Degrease acetone or alcohol. You will need splinters of any porcelain subject. Take mortar and pestle and their istolkita in powder. Cover chip with epoxy glue and strew with porcelain powder. Add chalk, talc or zinc white. Level and give to harden within 2 hours. Then grind and polish the repaired surface.

4. One more easy and cheap way of repair of enamel covering. Clean the place of chip with gasoline. Degrease, dry. Mix BF-2 glue and dry zinc white or Supertsement and nitroenamel to consistence of sour cream. Apply on the place of chip of 3-5 layers with interval of 1-2 hours. The surface turns out smooth and strong. For full hardening it is required four days - it is the only lack of this method.